When laying a brick on a cement- sand- mortar, the air temperature should not fall below plus 5C Not in the daytime or nighttime, at the time of the droping the rule can destroy the chemical. Process,which results in solubility and extinction For the laying of walls from large-format-blocks with negative should be applied solutions withChemical antifreeze additives, a solution for work at a temperature of up to 10C When laying,u can not use frozen bricks or bricks on the surface,which have snow or ice It is imortant to cover the surface of the sillsşwalls,watertight covers that will protect the masonry from rain inside the voids In the heat at temperature of ,more than 25C it is recommended to wet ceramic bloks with water, before laying Follow the simple rules,and your walls will serve for a centuries.